<?xml version="1.0" encoding="UTF-8"?>

<?xml-stylesheet type="text/xsl" href="/static/oaitohtml.xsl"?>

<!--
<?xml-stylesheet type="text/xsl" href="/oaitohtml.xsl"?>
-->

<OAI-PMH xmlns="http://www.openarchives.org/OAI/2.0/" xsi:schemaLocation="http://www.openarchives.org/OAI/2.0/ http://www.openarchives.org/OAI/2.0/OAI-PMH.xsd" xmlns:xsi="http://www.w3.org/2001/XMLSchema-instance">
    <responseDate>2026-10-13T23:06:54Z</responseDate>
    <request verb="GetRecord" metadataPrefix="oai_dc" identifier="10.57760/sciencedb.03567" >https://www.scidb.cn/oai</request>
<GetRecord>
    <record>
    <header >
    <identifier>10.57760/sciencedb.03567</identifier>
    <datestamp>2022-10-20T10:28:28Z</datestamp>
</header>
    <metadata>
        
<oai_dc:dc xmlns:oai_dc="http://www.openarchives.org/OAI/2.0/oai_dc/" xmlns:dc="http://purl.org/dc/elements/1.1/" xmlns:xsi="http://www.w3.org/2001/XMLSchema-instance" xsi:schemaLocation="http://www.openarchives.org/OAI/2.0/oai_dc/ http://www.openarchives.org/OAI/2.0/oai_dc.xsd">
  <dc:date>2022-10-20</dc:date>
  <dc:title>Deuterium retention and surface morphology modification in oxidized tungsten exposed to D plasma</dc:title>
  <dc:identifier>doi:10.57760/sciencedb.03567</dc:identifier>
  <dc:language>en</dc:language>
  <dc:description>本文的数据由SEM（扫描电镜）、GIXRD（掠角X射线衍射）和TDS（热脱附谱）组成，其中SEM分析完成于淮南新能源研究中心、GIXRD完成于中科院固体物理研究所、TDS完成于中科院等离子体物理研究所。</dc:description>
  <dc:subject>deuterium retention; plasma facing material; oxide tungsten</dc:subject>
  <dc:creator>Puyang Shouan</dc:creator>
  <dc:creator>Lv Yiming</dc:creator>
  <dc:creator>Nian Feifei</dc:creator>
  <dc:creator>Xu Yuping</dc:creator>
  <dc:creator>Yang Zhongshi</dc:creator>
  <dc:creator>Zhou Haishan</dc:creator>
  <dc:creator>Luo Guangnan</dc:creator>
  <dc:rights>PUBLIC</dc:rights>
  <dc:rights>https://creativecommons.org/publicdomain/zero/1.0/</dc:rights>
  <dc:type>dataset</dc:type>
  <dc:publisher>Science Data Bank</dc:publisher>