<?xml version="1.0" encoding="UTF-8"?>

<?xml-stylesheet type="text/xsl" href="/static/oaitohtml.xsl"?>

<!--
<?xml-stylesheet type="text/xsl" href="/oaitohtml.xsl"?>
-->

<OAI-PMH xmlns="http://www.openarchives.org/OAI/2.0/" xsi:schemaLocation="http://www.openarchives.org/OAI/2.0/ http://www.openarchives.org/OAI/2.0/OAI-PMH.xsd" xmlns:xsi="http://www.w3.org/2001/XMLSchema-instance">
    <responseDate>2026-10-14T12:19:16Z</responseDate>
    <request verb="GetRecord" metadataPrefix="oai_dc" identifier="10.57760/sciencedb.13407" >https://www.scidb.cn/oai</request>
<GetRecord>
    <record>
    <header >
    <identifier>10.57760/sciencedb.13407</identifier>
    <datestamp>2024-09-25T16:37:00Z</datestamp>
</header>
    <metadata>
        
<oai_dc:dc xmlns:oai_dc="http://www.openarchives.org/OAI/2.0/oai_dc/" xmlns:dc="http://purl.org/dc/elements/1.1/" xmlns:xsi="http://www.w3.org/2001/XMLSchema-instance" xsi:schemaLocation="http://www.openarchives.org/OAI/2.0/oai_dc/ http://www.openarchives.org/OAI/2.0/oai_dc.xsd">
  <dc:date>2024-09-25</dc:date>
  <dc:title>The role of oligomeric poly(-caprolactone)-diol and Laponite addition on biodegradability, anti-fouling, mechanical properties, organic dye, and heavy metal ion adsorption of PCL porous membrane</dc:title>
  <dc:identifier>doi:10.57760/sciencedb.13407</dc:identifier>
  <dc:language>en</dc:language>
  <dc:description>Biodegradable polymeric membranes for water treatment and desalination could help mitigate the environmental impact of polymeric waste from discarded membranes. In this context, poly(&amp;epsilon;-caprolactone) (PCL) is a promising choice, but its hydrophobicity limits salt and water contaminant adsorption. To address these issues, PCL was blended with oligomeric PCL-diol (PCL-D) in ratios of 90:10, 80:20, and 70:30, and further 12 wt% Laponite (Lap), an anionic synthetic hectorite clay, was incorporated to the above blends to impart functionality and mechanical stiffness. The addition of PCL-D improved the porosity, hydrophilicity, and antifouling properties, while Lap enhanced mechanical properties and functionality vis-&amp;agrave;-vis the above properties. Notably, the pure water flux (PWF) increased from ~188 Lm⁻&amp;sup2;h⁻&amp;sup1; for neat PCL to 1124 Lm⁻&amp;sup2;h⁻&amp;sup1; for the 70:30 PCL:PCL-D blend with 12 wt% Lap (P7D3-L12), and the water contact angle (WCA) decreased from ~96&amp;deg; to ~49&amp;deg;. The membranes showed excellent desalination and adsorption of heavy metal ions and organic dyes. The P7D3-L12 membrane had an adsorption capacity of ~45 mg/g for MB, ~57 mg/g for NR dye, ~84.9 mg/g for Pb&amp;sup2;⁺, and ~90.6 mg/g for Cd&amp;sup2;⁺. It also achieved 35.6% and 39.8% salt retention for NaCl and Na₂SO₄ after 4 cycles. The fouling recovery rate (FRR) for the P7D3-L12 membrane was ~93% after the 1st cycle and ~82% after the 5th cycle. The P7D3-L12 membrane showed 78% weight loss in compost over 54 days, highlighting its improved biodegradability. Thus, these modified membranes offer a promising biodegradable solution for water treatment and desalination.</dc:description>
  <dc:subject>Poly(-caprolactone); porous membrane; Laponite; biodegradation; desalination; dye adsorption</dc:subject>
  <dc:creator>Divyansh Upreti</dc:creator>
  <dc:creator>Chitransh Upreti</dc:creator>
  <dc:creator>T Umasankar Patro</dc:creator>
  <dc:rights>PUBLIC</dc:rights>
  <dc:rights>https://creativecommons.org/licenses/by-nc-nd/4.0/</dc:rights>
  <dc:type>dataset</dc:type>
  <dc:publisher>Science Data Bank</dc:publisher>
</oai_dc:dc>

    </metadata>
</record>
</GetRecord>
</OAI-PMH>