<?xml version="1.0" encoding="UTF-8"?>

<?xml-stylesheet type="text/xsl" href="/static/oaitohtml.xsl"?>

<!--
<?xml-stylesheet type="text/xsl" href="/oaitohtml.xsl"?>
-->

<OAI-PMH xmlns="http://www.openarchives.org/OAI/2.0/" xsi:schemaLocation="http://www.openarchives.org/OAI/2.0/ http://www.openarchives.org/OAI/2.0/OAI-PMH.xsd" xmlns:xsi="http://www.w3.org/2001/XMLSchema-instance">
    <responseDate>2026-10-13T22:59:46Z</responseDate>
    <request verb="GetRecord" metadataPrefix="oai_dc" identifier="10.57760/sciencedb.j00124.00089" >https://www.scidb.cn/oai</request>
<GetRecord>
    <record>
    <header >
    <identifier>10.57760/sciencedb.j00124.00089</identifier>
    <datestamp>2024-11-21T14:43:44Z</datestamp>
</header>
    <metadata>
        
<oai_dc:dc xmlns:oai_dc="http://www.openarchives.org/OAI/2.0/oai_dc/" xmlns:dc="http://purl.org/dc/elements/1.1/" xmlns:xsi="http://www.w3.org/2001/XMLSchema-instance" xsi:schemaLocation="http://www.openarchives.org/OAI/2.0/oai_dc/ http://www.openarchives.org/OAI/2.0/oai_dc.xsd">
  <dc:date>2024-11-21</dc:date>
  <dc:title>A dataset for the preparation of Fe/SAPO-34 catalyst and its performance in CO hydrogenation to low-carbon olefins</dc:title>
  <dc:identifier>doi:10.57760/sciencedb.j00124.00089</dc:identifier>
  <dc:language>en</dc:language>
  <dc:description>The X-ray diffraction (XRD) pattern was analyzed and recorded on Advance (Bruker AXS) using Cu K &amp;alpha; as the radiation source. The texture properties and pore size distribution information were obtained on the JW-BK200 physical adsorption instrument. Scanning electron microscopy (SEM) was used for observation and analysis on JSM-7900F. XRF was measured on a Thermo Fisher XRF-3600 X-ray fluorescence spectrometer. NH3 temperature programmed desorption (NH3-TPD) was measured on a TP-5080 adsorbent. CO temperature programmed desorption (CO-TPD) and H2 temperature programmed desorption (H2-TPD) were tested on the BELCAT II catalyst analyzer. In situ infrared (DRIFTS) characterization was performed on a Bruker Vertex 80v FTIR spectrometer. XPS was collected on an ESCALAB 250Xi photoelectron spectrometer and calibrated based on a C 1s binding energy of 284.80 eV.&amp;nbsp;</dc:description>
  <dc:subject>XRD; N2 physisorption; SEM; TEM; XPS; NH3-TPD; H2-TPD; CO-TPD; In situ infrared; Performance evaluation data; reaction mechanism</dc:subject>
  <dc:creator>Li Liuliu</dc:creator>
  <dc:creator>Fang Kegong</dc:creator>
  <dc:creator>Zhang Mingwei</dc:creator>
  <dc:creator>Wang Yingjun</dc:creator>
  <dc:rights>PUBLIC</dc:rights>
  <dc:rights>https://opendatacommons.org/licenses/by/1-0/</dc:rights>
  <dc:type>dataset</dc:type>
  <dc:relation>http://www.doi.org/10.1016/s1872-5813(24)60505-0</dc:relation>
  <dc:publisher>Science Data Bank</dc:publisher>
</oai_dc:dc>